New nickel-base superalloys enables more efficient gas turbines

News and results from the project Weldability of nickel-base superalloys for energy applications, KME-706.
KME706.png

The most important project results are weldability data for the relatively new superalloys Haynes282 and 718Plus. The data enables a comparison to the ‘standard’ grade Alloy718 and can provide the necessary information for material selection for hot structural parts in gas turbine engines. The application of alloys with increased maximum service temperature such as the two above-mentioned ones could be used to make the combustion process in aircraft engines more efficient. This generally affects gas turbine manufacturers as well as companies involved in the process as a supplier of either the material or manufactured parts.

The tolerance towards a higher service temperature however often goes hand in hand with increased risk for cracking during welding, specifically via a mechanism called strain age cracking. This cracking phenomenon is unique for precipitation hardening superalloys and occurs during the heating towards post weld heat treatment, which is used to obtain uniform material properties after welding. Profound knowledge of the ongoing mechanisms is key to avoid failure and can be obtained via different test methods such as the one developed within this project, which provides information on the performance of microstructures close to those present in real weld heat affected zones.

During the last year of the project more results will be obtained for 718Plus regarding its repair weldability, supplementing the already available data on the alloy’s weldability. Furthermore, a newly developed testing procedure using the Gleeble thermomechanical simulator will be used to characterize the resistance of Haynes 282 towards strain age cracking and to obtain a deeper knowledge on the ongoing mechanisms, which adds to the already obtained results that show the actual material performance.

It was unexpected to find no cracks in the base metal heat affected zone after repair welding Haynes 282 when examining over 100 weld cross sections.

The picture above shows:
General mechanism of strain age cracking. Fast heating and cooling during the weld thermal cycle, followed by slow heating to post weld heat treatment, where stress relaxation coincides with precipitation of hardening phases and intergranular cracking occurs.

Deformation behaviour of Haynes 282 tested at different temperatures. More brittle behaviour indicates temperature range with higher risk for strain age cracking.

Gleeble thermomechanical simulator that is used for weldability testing.

Different voids found in repair welded Haynes282. Left: Solidification crack. Right: Crack-like oxide inclusion between weld deposit layers.

PhD students, project participants and project leader of project:
Lars Nyborg (Project leader and assistant supervisor, Chalmers University of Technology)
Joel Andersson (Main supervisor, University West)
Fabian Hanning (PhD Student, Chalmers University of Technology)
Bengt Pettersson (Materials Expert, GKN)
Johan Ockborn (Welding Expert, GKN)

Participating companies:
GKN Aerospace Sweden AB

To the project-site.

Aktuellt

Lärorika FoU-dagar i Karlstad
Gammalkroppa fiskodling
  • Nyheter
Så kan vätgasens roll i energisystemet se ut – beroende på utvecklingsväg
Så kan vätgasens roll i energisystemet se ut – beroende på utvecklingsväg
  • Nyheter
  • Energisystem
Liten prispåverkan av produktionsstöd – men utformningen kan slå hårt mot statskassan
Anders Kofoed-Wiuff
  • Nyheter
  • Energisystem
Osäkerheten kring litiumjonbatterier bromsar säker energilagring
Nyhet, Batterienergilagring i litiumjonbatterier.jpeg
  • Nyheter
  • Elnät
Elpris och lokalisering påverkar framtidens vätgasvärdekedjor och infrastruktur
Bild Elpris och lokalisering påverkar framtidens vätgasvärdekedjor och infrastruktur
  • Nyheter
  • Energisystem