KME-HTC Symposium 2017
Opening
Chairperson: Bo Jönsson
Presentation of the KME programme - one year left
Bertil Wahlund, Energiforsk
Presentation of HTC – towards a new contract period
Lars-Gunnar Johansson, Chalmers
Steam boiler applications
Critical corrosion phenomena in the combustion of biomass and waste
Introduction
Jesper Liske, Chalmers
The effect of chlorine containing salts and HCl(g) on waterwall corrosion (HTC)
Amanda Persdotter, Chalmers
The effect of Cr and Si on FeCrAl model alloys (HTC)
Johan Eklund, Chalmers
Chairperson: Sven Andersson
High Temperature corrosion in small scale biomass boilers (HTC)
Bo Jönsson, Sandvik Heating Technologies
Keynote 1:
High Temperature Corrosion by Molten Nitrates in Concentrated Solar Power Plants
Mathias Galetz, Dechema Forschungsinstitut
High temperature corrosion in used wood fired boilers (KME-708)
Pamela Henderson, Vattenfall
High temperature corrosion in used wood fired boilers fuel additives and coatings (KME-718)
Annika Talus, Swerea KIMAB
Boiler corrosion at lower temperatures – influence of lead, zinc and chlorides found in used wood (KME-717)
Rickard Norling, Swerea KIMAB
Increased steam temperature in grate fired boilers - Steamboost (KME-709)
Loli Paz & Torbjörn Jonsson, Chalmers
Chairperson: Pamela Henderson
Combating superheater corrosion by new materials and testing procedures (KME-711+KME-720)
Andrea Olivas & Jesper Liske, Chalmers
Sulphur recirculation and improved material selection for high temperature corrosion abatement (KME-714)
Julien Phother & Loli Paz, Chalmers
Strain age cracking in nickel based superalloys (KME-706)
Hot cracking in high temperature materials (KME-719)
Fabian Hanning & Sukhdeep Singh, Chalmers
Materials challenges in new energy technologies
Chairperson: Anna Jonasson
Composite Metal Polymer for non-stick improvements in CHP plants (KME-715)
Rikard Norling, Swerea-KIMAB
Improved steam turbine design for optimum efficiency and reduced cost of ownership (KME-707)
Srikanth Deshpande, LU
Influence of high-temperature environments on the mechanical behaviours of high-temperature austenitic stainless steel (KME-701)
Hugo Wärner, LiU
Design of a new generation of 12 % chromium steels (KME-710)
Masoud Rashidi, Chalmers
Chairperson: Dilip Chandrasekaran
Corrosion of FeCr alloys in Solid Oxide Fuel Cells (SOFC) (HTC)
Claudia Goebel, Chalmers
High Temperature Corrosion in Gasification of Biomass and waste (HTC)
Rikard Norling, Swerea KIMAB
High temperature materials for industrial processes (HTC)
Christine Geers & Nooshin Mortazawi, Chalmers
Gas turbine applications
Chairperson: Marie-Aude Porter
Keynote 2:
The interaction between Stress and Corrosion at High Temperatures
John Nicholls, Cranfield University
High temperature corrosion in gas turbines (HTC)
Anand Harihara, Chalmers/GKN
LCF and TMF crack growth in cast nickel-base superalloys (KME-702)
Johan Moverare, LiU
Durable MCrAlX Coatings for demanding applications in gas turbines (KME-703)
Pimin Zhang, LiU
MoSi2 matrix composites for combustion components exposed to high temperature oxidation and hot corrosion (KME-705)
Erik Ström, Sandvik HT
High Temperature Corrosion of Nickel Base Alloys in a H2O/CO2 Gas Environment
Mohammad Sattari & Mats Halvarsson, Chalmers