KME-HTC Symposium 2018
Opening and chairperson: Bosse Jönsson, Kanthal/Chalmers
KME – 20 years of research and next programme stage
Bertil Wahlund, Energiforsk
HTC – the new contract period
Lars-Gunnar Johansson, Chalmers
Key note lecture
Effect of Pressure on Metal Dusting Initiation in CO-rich Syngas
Mathias Galetz, Dechema Forschungsinstitut
Steam boiler applications
High temperature corrosion in used wood fired boilers fuel additives and coatings (KME-708 and KME-718)
Annika Talus, Swerea KIMAB
Boiler corrosion at lower temperatures – influence of lead, zinc and chlorides found in used wood (KME-717)
Rikard Norling, Swerea KIMAB
Composite Metal Polymer for non-stick improvements in CHP plants (KME-715)
Ragna Elger, Swerea KIMAB
Chairperson: Anna Jonasson, EON
Critical corrosion phenomena in the combustion of biomass and waste (HTC)
Introduction
Jesper Liske, Chalmers
The effect of the amount of KCl on the mode of corrosion
Julien Phother, Chalmers
High temperature chlorine-induced corrosion of low-alloyed and stainless steel – The role of oxide scales
Andrea Olivas, Chalmers
The effect of Cr and Si on FeCrAl model alloys in KCl environments
Johan Eklund, Chalmers
Increased steam temperature in grate fired boilers - Steamboost (KME-709)
Loli Paz & Torbjörn Jonsson, Chalmers
Corrosion of high temperature materials in burners and boilers for small-scale combustion of biomass (HTC)
Carolina Pettersson, Swerea IVF
Chairperson: Pamela Henderson, Vattenfall
Sulphur recirculation and improved material selection for high temperature corrosion abatement (KME-714)
Loli Paz & Torbjörn Jonsson, Chalmers
Combating superheater corrosion by new materials and testing procedures (KME-711+720)
Andrea Olivas & Jesper Liske, Chalmers
Materials challenges in energy technologies
Chairperson: Dilip Chandrasekaran, Kanthal
Influence of high-temperature environments on the mechanical behaviours of high-temperature austenitic stainless steel (KME-701)
Mattias Calmunger, LiU
Design of a new generation of 12 % chromium steels (KME-710)
Fang Liu, Chalmers
High Temperature Corrosion in Gasification of Biomass and waste (HTC)
Rikard Norling, Swerea KIMAB
High temperature materials for industrial processes (HTC)
Christine Geers, Chalmers
Corrosion of FeCr alloys in Solid Oxide Fuel Cells (SOFC) (HTC)
Claudia Göbel, Chalmers
Steam and Gas turbine applications
Chairperson: Lars-Gunnar Johansson, Chalmers
High temperature corrosion in gas turbines (HTC)
Anand Harihara, Chalmers
LCF and TMF crack growth in cast nickel-base superalloys (KME-702)
Daniel Leidermark, Frans Palmert & Christian Busse, LiU
Durable MCrAlX Coatings for demanding applications in gas turbines (KME-703/713)
Pimin Zhang, LiU
Strain age cracking in nickel based superalloys (KME-706)
Hot cracking in high temperature materials (KME-719)
Fabian Hanning & Sukhdeep Singh, Chalmers
MoSi2 matrix composites for combustion components exposed to high temperature oxidation and hot corrosion (KME-705)
Erik Ström, Kanthal
High Temperature Corrosion of Nickel Base Alloys in a H2O/CO2 Gas Environment (HTC)
Mats Halvarsson, Chalmers